Sodium Dichromate 1lb Enhanced Gypsums Adjust the concentration based on
Pay in 4 interest-free payments of $19.00 Learn more
Shipping Estimate
USA
- USA
- CAN
- USA
- CAN
Ships within 48 hours · Estimated delivery Jul 31 - Aug 5
Live Spec
Sodium Dichromate 1lb Enhanced Gypsums Adjust the concentration based onCreating a patina with sodium dichromate typically involves making a solution with water and applying it to metals such as brass or bronze. To prepare the solution, you would dissolve a small amount of sodium dichromate in water. The ratio can vary, but as a general guideline, you might start with about a teaspoon of sodium dichromate per liter of water. Adjust the concentration based on the desired effect. Apply the solution to the metal surface